Ive been trying to get my 3D printer to print properly since upgrading my Ender 3 Pro with an all metal direct drive hot end. I calibrated my esteps perfectly and they're spot on, beds leveled although there is a bit of a dip in the middle, and my slicer has the right settings for this PLA that is new and just opened from the air tight bag. Not sure why im getting these weird first layers.
Slicer settings:
200c hot end
60c bed
50mm/s
Filament recommendations
190-220c hot end
25-70c bed
50mm/s
Looks like it's got a jam. Did you reduce retractions with the direct hotend? If not, you are probably retracting way too far, which will cause filament to solidify in the cold area and jam up.